Welcome to Chemistry and Industry of Forest Products,

Chemistry and Industry of Forest Products ›› 2015, Vol. 35 ›› Issue (6): 83-88.doi: 10.3969/j.issn.0253-2417.2015.06.014

Previous Articles     Next Articles

Synthesis and Properties of Hydrogenated Rosin Modified Vinyl Polysiloxane

XU Tao1,2, LIU He1, SHANG Shi-bin1, SONG Zhan-qian1, YANG Chong2   

  1. 1. Institute of Chemical Industry of Forest Products, CAF; National Engineering Lab.for Biomass Chemical Utilization; Key and Open Laboratory of Forest Chemical Engineering, SFA; Key Lab.of Biomass Energy and Material, Jiangsu Province; Nanjing 210042, China;
    2. Shenzhen Guanheng New Materials Technology Co., Ltd, Shengzhen 518109, China
  • Received:2014-09-23 Online:2015-12-25 Published:2015-12-28

Abstract: Hydrogenated rosin (HR) modified vinyl polysiloxane (HR-VMS) was firstly synthesized from HR, hexamethyldisiloxane (MM), 1, 3, 5, 7-tetravinyl-1, 3, 5, 7-tetramethylcyclotetrasiloxane (D4Vi), octamethyl cyclotetrasiloxane (D4) and hydrolyzate of γ-aminopropyl(diethoxy)methylsilane (HAPMS).The novel resin (HR-VMS) was further characterized by 1H NMR, 13C NMR and FT-IR.The curing behavior of HR-VMS with 2, 5-bis(tert-butylperoxy)-2, 5-dimethylhexane(DBPH) as the curing agent was studied by differential scanning calorimetry (DSC).The low-temperature resistance and high-temperature thermal stability of the curing product were studied by DSC and TG, respectively.The results showed that at the heating rate of 10℃/min, the peak-top temperature of exothermic peak for HR-VMS was 186.9 ℃ with the exothermic value of 100.3 J/g.The curing product from HR-VMS showed better high-temperature thermal stability compared with VMS, and the temperature corresponding to its maximum weight loss rate was 436.1℃ which was 68℃ higher than that of common vinyl polysiloxane resin.

Key words: hydrogenated rosin, modification, poly(dimethylsiloxane), peroxide, sulfurization